Superalloy Hastelloy C276 C22 C4 B2 X Monel 400 K500 Inconel 600 601 625 718 Incoloy 800 800h 925 926 Alloy Nickel Steel Coil/Strip/Plate/Sheet Nickel Alloy
Basic Info.
Model NO. | Nickel Alloy Series |
Transport Package | as Required |
Specification | Support Customization |
Trademark | Shanghai Century Dongrui Steel Co., Ltd. |
Origin | Wuxi City, China |
HS Code | 72193400 |
Production Capacity | 50000piecs/Year |
Product Description
Nickel base alloys: Incoloy800 (1.4558), Incoloy800H, Incoloy825 (2.4858), inconel600 (2.4817), n06601 (2.4851), inconel690 (2.4642), Hastelloy B, Hastelloy B-2 (2.4617), Hastelloy C, Hastelloy C-276 (2.4819), Hastelloy C-4 (2.461), Inconel625 (2.4856)
Greetings! Are you looking for a supplier of stainless steel pipes? We are capable to fulfill your need and achieve the highest customers satisfaction at the most reasonable price. Integrity and high efficiency is our service tenet, we dedicated to providing excellent products and service to new and old customers. Feel free to contact us if you are:· Looking for high-quality steel products or have special specifications.· Have a special and/or large demand for steel products and seeking a long-term supplier.· An international user, retailor, wholesaler of steel products.· Looking for professional customer service with high responsibilityTest | UT, ET, HT, RT,ect, and others according to the standard,or as the requests of the customers | |
Standard |
| |
ASTM, GB, JIS, DIN, EN, AISI | ||
Material Grade |
| |
TP410 TP410S TP430 | ||
S31803/S32205 S32750 S32760 | ||
Certificate | ISO9001-2008,ASME, PED | |
Delivery Time | 3-25 Days, Depends on quantity |
Chemical composition
Margin Chromium Cr: 0.4~0.7 iron Fe: 1.6 ~ 2.0 Carbon C: 0.01 Manganese Mn: 1.0 Silicon Si: 0.08 Copper Cu: 0.5 Molybdenum Mo: 26.0~30.0 Cobalt Co: 1.0 Phosphorus P: 0.02 Sulfur S:0.01
Hastelloy B-2 physical properties
Hastelloy B-2 density
• Density ρ=9.2g/cm3
• HastelloyB-2 melting temperature range
• Melting temperature range 1330~1380°C
• Hastelloy B-2 welding
• The Hastelloy B-2 can be welded with tungsten electrode shielded gas (GTAW/TIG) or gas shielded arc welding (SMAW/MMA) in certain environments.
• The material to be welded should be annealed, remove oxide scale, oil and various marking marks, and the area of the base metal on both sides of the weld about 25mm wide must be polished to a bright metal.
• Hastelloy B-2 has a lower thermal conductivity than steel, and when using a single V-weld interface, the angle should be 70°, with a low heat input, and the interlayer temperature should not exceed 120°C.
• The oxidation color can be brushed off when the weld is still hot.
• Post-weld heat treatment is required in some applications to eliminate residual stress and improve stress corrosion cracking resistance.
• In order to obtain good corrosion resistance, it is recommended to use argon arc welding, that is, tungsten electrode inert gas shielded welding GTAW.
FAQ: Q: Are you trading company or manufacturer ?A: We are Manufacturing and processing enterprises
Q: How many countries you already exported?
A: Exported to more than 25 countries mainly from Brazil,India, Russia, UK, Vietnam, Egypt, Turkey, Saudi Arabia, Dubai etc
Q: How long will it take to execute my order?
A: Our normal time to execute the order is 7-20 working days. We will let you know the estimated lead time after Payment ASAP
Q: Can I have a sample for testing?
A: Free samples, you just need to pay the freight
Q:Do you have inspection for the products before packing?
A: 100% self-inspection for the products, we put the quality as our first priority.Q :Can I have a visit to your factory before the order?
A: Sure, welcome to visit our factory.